S355JR vs S355J2: What Impact Test Temperature Means for Charpy

Akuracy Charpy impact testing machine RI 300 for S355 structural steel impact tests

Ameet Kudche |

Short answer: in EN 10025-2 structural steel, the letters after S355 tell you how the Charpy V-notch impact test is done. S355JR must absorb at least 27 J at +20 °C (room temperature). S355J0 must absorb 27 J at 0 °C. S355J2 must absorb 27 J at −20 °C, and S355K2 needs 40 J at −20 °C. The yield strength is the same, so the only difference between JR and J2 is toughness at low temperature. That changes how the test lab has to prepare, cool and break the specimens.

Akuracy Charpy impact testing machine RI 300 for S355 structural steel impact tests

Decoding the S355 designation

  • S = structural steel.
  • 355 = minimum yield strength in MPa for the thinnest thickness range.
  • J / K = the minimum impact energy: J means 27 J and K means 40 J.
  • R / 0 / 2 = the test temperature: R is room temperature (+20 °C), 0 is 0 °C and 2 is −20 °C.
Grade Test temperature Minimum impact energy (Charpy V, longitudinal)
S355JR +20 °C 27 J
S355J0 0 °C 27 J
S355J2 −20 °C 27 J
S355K2 −20 °C 40 J

The minimum applies to the average of a set of three specimens. The product standard also has a rule for how far a single specimen may fall below the minimum. Check the edition named on the mill certificate or purchase order.

Why the test temperature matters

Ferritic steels go through a ductile-to-brittle transition as temperature drops. At room temperature most S355 breaks in a ductile way and absorbs plenty of energy. As the temperature falls, the fracture becomes more brittle and the absorbed energy drops sharply. A J2 grade is guaranteed to stay above 27 J at −20 °C, which matters for outdoor structures, cranes, bridges, offshore and cold-climate equipment. A JR grade only promises toughness at room temperature, and it may fall below 27 J at −20 °C.

Indian equivalent: IS 2062 sub-qualities

IS 2062 uses a similar idea with sub-qualities A, BR, B0 and C. Quality A needs no impact test. BR is tested at room temperature (the test is optional unless ordered), B0 is tested at 0 °C and C at −20 °C. For grades such as E250 and E350, the required minimum is 27 J. So in terms of test temperature, E350C is broadly comparable to S355J2. Chemistry, thickness ranges and other limits still differ, so do not treat the two as interchangeable without checking both standards.

How the lab runs a −20 °C Charpy test

  1. Machine and notch: standard 10 × 10 × 55 mm specimens with a 2 mm V-notch, prepared on a broaching or milling setup and checked with a notch gauge or profile projector.
  2. Cooling: specimens are soaked in a controlled liquid bath (for example alcohol cooled by a chiller or dry ice) at the test temperature for the time the standard specifies.
  3. Transfer: each specimen is moved from the bath to the anvil and broken within about five seconds, as the standard specifies, so it does not warm up. Self-centring tongs make this quicker and more repeatable.
  4. Recording: absorbed energy for each specimen, plus lateral expansion and shear fracture appearance if the customer requires them.

The biggest source of false failures is the specimen warming during a slow transfer. The second is a poorly finished notch.

Choosing impact testing equipment

A structural steel lab needs a pendulum Charpy machine with enough energy for tough specimens at room temperature, a notch preparation machine, a notch gauge and a low-temperature bath. Akuracy's Charpy impact testing machine RI 300 lists a caliper gauge for V-notch verification and self-centring tongs. The RI 300 E supports both Charpy and Izod tests. See all options in the impact testing machine range.

Common reasons S355J2 fails at −20 °C

  • Specimen warmed during transfer (too slow, or tongs not pre-cooled).
  • Notch radius or depth out of tolerance.
  • Specimens taken in the wrong orientation (transverse instead of longitudinal, or the other way round).
  • Material really is JR quality supplied against a J2 order. Verify the mill certificate.

Where this matters in industry

Steel stockists re-certify plates for project orders. Fabricators of cranes, towers, bridges and pressure-part supports verify incoming steel. Third-party labs issue Charpy reports for export orders that specify EN grades. In all of these, a J2 or K2 requirement means the lab must be able to test reliably at −20 °C.

FAQ

What is the impact test temperature for S355J2?

−20 °C, with a minimum of 27 J average absorbed energy on Charpy V-notch specimens.

What is the impact test temperature for S355JR?

+20 °C (room temperature), with a minimum of 27 J.

Is S355J2 stronger than S355JR?

No. Both have the same minimum yield strength. J2 is guaranteed to be tougher at −20 °C.

Can S355J2 replace S355JR?

Generally yes, because it meets a stricter toughness requirement. Replacing J2 with JR is not acceptable without approval.

What does K2 mean?

A minimum of 40 J at −20 °C, which is stricter than J2.